当前位置:首页> 新闻中心>新闻资讯>怎么处理锈石出现水斑的情况?
怎么处理锈石出现水斑的情况?
来源:http://www.shengyashicai.com 日期:2019-06-04 发布人:admin
 浏览量:
  黄锈石水斑管理剂的运用。黄锈石水斑管理剂油两种药剂组成,分为A剂、B剂,对不同黄锈石水斑,药剂的投入量是变化的,总的准绳是水斑的时间越长,斑色越黑,药剂投入时应越多。初次施工约剂的投入量也应增大投放时。随着水斑的颜色变浅,药剂的投入量也应减少。药剂的注入量应控制这样一个准绳“先重后轻”。先重后轻的准绳也应停止一些小的调整,这请求施工人员应有一定施工经历,在药剂的注入量上要有很好的把握。假如可以很好地控制办法,黄锈石水斑这个“癌症”还是能够管理。
  Application of yellow rust plaque management agent. There are two kinds of reagents in yellow rust plaque management agent oil, which are A and B. For different yellow rust plaques, the dosage of reagent is changing. The general criterion is that the longer the time of water plaque is, the darker the spots are, the more the reagent should be put in. Initial construction agent input should also be increased. As the color of water spots becomes lighter, the dosage of medicines should also be reduced. The dosage of medicines should be controlled according to such a criterion as "weighting first and then lightening". The first priority criterion should also stop some minor adjustments, which requires that the construction personnel should have a certain construction experience and have a good grasp of the amount of medicines injected. If it can be well controlled, the "cancer" of yellow rust plaque can still be managed.
  1、清洗管理法:运用强酸涂刷于黄锈石外表,为使注入大量加大,运用敷盖黄锈石水斑。此办法是不可取的。一方面强酸会和黄锈石内部的矿物发作反响,会腐蚀黄锈石外表另一方面,大量酸性湿斑,这一类酸性湿斑也是不容易肃清的。
  1. Cleaning management method: apply strong acid to coat the surface of yellow rust stone. In order to increase the injection, apply the coating to cover the yellow rust water spot. This method is not advisable. On the one hand, strong acid will react with the minerals inside the yellow rust stone, which will corrode the appearance of the yellow rust stone. On the other hand, a large number of acid wet spots, which are not easy to remove.
山东锈石厂
  2、加热法:运用喷灯或高温灯停止烘烤。
  2. Heating: Stop baking with a blowtorch or high-temperature lamp.
  此办法去除黄锈石水斑,在短时间会有一点效果,但在施工后一段时间内,水斑会恢复到原来的情况,并且,假如黄锈石底面防护剂运用不当,经过烘烤还会形成黄锈石的空鼓。由于此办法会产生不可补偿的结果,不倡议采用。
  This method can get some effect in a short time, but within a period of time after construction, the water spots will return to the original situation. Moreover, if the protective agent for the bottom of the yellow rust stone is improperly used, the hollow drum of the yellow rust stone will be formed after baking. As this approach will produce irreparable results, it is not advocated.
  3、综合药剂管理法:综合药剂管理是充沛的思索了黄锈石水斑构成的机理及不同黄锈石水斑的实践状况,而采取的管理办法。下面分离我们的运用综合药剂管理黄锈石水斑停止讨论:
  3. Comprehensive Pharmaceutical Management Method: Comprehensive Pharmaceutical Management is the management method adopted by abundant thinking about the mechanism of the formation of yellow rust stone water spots and the practical situation of different yellow rust stone water spots. Next, we separated our discussion on the application of comprehensive medicines in the management of yellow rust spots.
  针对不同状况产生的水斑,管理剂应采用不同的施工程序,没有停止过黄锈石外表防护的黄锈石,只需将黄锈石外表的尘土清洗洁净,就可涂刷管理剂。
  For different water spots, the admixture should adopt different construction procedures. It has not stopped the rust stone which has been protected by the appearance of the rust stone. Only the dust on the surface of the rust stone can be cleaned and cleaned, and the admixture can be painted.