  如何控制山东锈石干湿抛光技术,我们都晓得山东锈石是一种自然石材,后期的加工能够使它的表面让更多的人喜欢山东锈石,干湿抛光可以让本来的山东锈石愈加有光泽,下面小编就这个问题的相关学问给大家整理了一篇文章让大家理解.
  How to control the dry-wet polishing technology of Shandong rust stone, we all know that Shandong rust stone is a kind of natural stone. Later processing can make its surface more people like Shandong rust stone. Dry-wet polishing can make the original Shandong rust stone more lustrous. Here is a short edition of the relevant knowledge on this issue for you to sort out an article. Let everyone understand.
  常见的山东锈石的抛光分为干抛光和湿抛光,抛光磨石在“干与湿”之间当石材产品发作物理化学作用,干抛光是在石材外表温度升高使水分蒸发,招致抛光磨石浓度增大,从而到达强化效果,产品光泽度开端到达了理想请求,光泽度达85度以上或更高。
  The polishing of common rust stones in Shandong Province is divided into dry polishing and wet polishing. When the physical and chemical effect of polishing millstone occurs between "dry and wet", dry polishing evaporates water and causes the concentration of polishing millstone to increase, so as to achieve the strengthening effect. The glossiness of the product reaches the ideal requirement at the beginning. The gloss is above 85 degrees or higher.
山东锈石厂
  抛光磨石在被加工产品上抛光,待抛光产品烫手后,将板面加水量水,以起到降温作用,不允许连续加水或大量加水,否则,水的光滑作用将会使抛光达不到理想效果,也不能全部运用干抛光,过高的温度会烧坏板面,而且会使板面呈现裂纹。普通而言,产品精磨后,产品的光泽度在40~50左右,而有些石材精磨后达不到上面的光泽度,如山西黑、黑金砂、集宁黑等,此类产品精磨后的光泽度只要20~30度之间,用前面的微粒研磨原了解释不够一面,这种产品在抛光“干与湿”,温度的升高,降温中,强化抛光过程,发作物理化学反响。
  Polishing whetstone polishes on the processed products. When the polished products are ironed, water is added to the surface of the plate to reduce the temperature. It is not allowed to add water continuously or in large quantities. Otherwise, the smooth effect of water will make the polishing not achieve the desired effect, and dry polishing can not be used completely. Excessive temperature will burn the surface of the plate, and it will also burn down. Cracks appear on the surface of the plate. Generally speaking, after finishing, the glossiness of products is about 40-50, while some stone materials can not reach the above glossiness after finishing, such as Shanxi black, black gold sand, Jining black, etc. The glossiness of such products after finishing is only between 20-30 degrees, which is not fully explained by the previous micro-grinding. This product is "dry" in polishing. With wet ", the increase of temperature, cooling, strengthening the polishing process, the occurrence of physical and chemical reactions.
  只需在加工山东锈石的时分像干湿抛光只需控制在上面的请求范围之内,就会使我们的山东锈石更具有质感,这样山东锈石的商业价值也会渐渐的进步,只需在做这些工作的时分把握好一些细节就能够了,希望上面的内容能够协助到大家.
  As long as the processing of Shandong rust stone like dry-wet polishing only needs to be controlled in the above request range, it will make our Shandong rust stone more textural, so that the commercial value of Shandong rust stone will gradually improve, just need to grasp some details when doing these work, I hope the above content can help. Everybody.